THERMO 600 PRIMER 有机硅耐热底漆600 属底漆。and other hot surfaces at temperatures up to 600℃and 650℃at a short time. 作为底漆长效保护温度高达600℃(瞬时温度650℃)的热管道、排气管、烟囱和其它热表面。由改性有机硅树脂与惰性颜料组成的耐热涂料。极好的耐热性(到600℃) Good weathering resistance 极好的耐候性 Good applicability 极好的施工性能。本页参数:体积固体份 45 ± 2%、干膜厚度 20-30 微米/道、理论涂布率 0.058 千克/平方米/20 微米。
以上内容整理自原厂说明书与本站参数表;选型、配套与货期请联系我们确认。
| 体积固体份 | 45 ± 2% |
|---|---|
| 干膜厚度 | 20-30 微米/道 |
| 理论涂布率 | 0.058 千克/平方米 /20 微米 |
| VOC | 550g/L |
| 密度/比重 | — |
| 组份数 | 单组份 |
| 闪点 | 27℃以上 |
| 稀释剂 | 稀释剂X |
| 混合比 | 单组份涂料 |
| THERMO 600 PRIMER | 有机硅耐热底漆600 |
|---|
A heat resisting paint based on modified silicone resin and inert pigments.
由改性有机硅树脂与惰性颜料组成的耐热涂料。
As a primer for long-term protection of hot pipelines, exhaust pipes, smoke stacks
and other hot surfaces at temperatures up to 600℃and 650℃at a short time.
作为底漆长效保护温度高达600℃(瞬时温度650℃)的热管道、排气管、烟 囱和其它热表面。
Excellent heat resistance (Up to 600℃)
极好的耐热性(到600℃)
Good weathering resistance
极好的耐候性
Good applicability
极好的施工性能
| Color | Black |
|---|---|
| 颜色 | 黑色 |
| Volume Solids 体积固体份 | 45±2% |
| Flash Point | Greater than 27℃ |
| 闪点 | 27℃以上 |
| VOC | 550g/L |
| 挥发性有机化合物含量 | 550g/L |
| Film thickness | Dry : 20-30 microns/coat Wet :44-67microns/coat |
| 涂装膜厚 | 干膜: 20-30 微米/道湿膜:44-67 微米/道 |
| Theoretical Coverage | 0.058kg/m²/20microns |
| 理论涂布率 | 0.058 千克/平方米/20 微米 |
Practical coverage depending on surface conditions, environment, applications, etc.
实际涂布率与表面处理, 外界环境, 施工方法等多种因素有关。
| Application Temperature 施工温度 | -5℃-40℃ |
|---|---|
| Mixing | Mix thoroughly with power agitator |
| 混合 | 使用动力工具搅拌均匀 |
| Mixing Ratio | One component coating |
| 混合比例 | 单组份涂料 |
| Application Methods | Airless spray, air spray, brush and roller |
| 施工方法 | 无气喷涂、空气喷涂、刷涂、滚涂 Airless spray 无气喷涂 |
| Nozzle tip | 喷嘴尺寸 | 0.33mm-0.43mm |
| Nozzle pressure | 出口压力 | ≥10Mpa |
| Thinning ratio | 稀释比率 | 0-5% by weight(重量比) |
Brush/Roller 刷涂、滚涂 Thinning ratio 稀释比率 0-5% by weight(重量比)
| Thinner | Paint Thinner X |
|---|---|
| 稀释剂 | 稀释剂X |
| Drying time & | Temperature | 温度 | 5℃ | 20℃ | 30℃ |
| Overcoating interval | Surface dry | 指触干燥 | 3hrs | 1hr | |
| 干燥时间&涂装间隔 | Touch dry | 半硬干燥 | 5hrs | 3hrs | |
| Min. interval | 最小涂装间隔 | 16hrs | 12hrs | 8hrs | |
| Max. interval | 最大涂装间隔 | ||||
Full cure: must bake in 200℃-250℃for 1hr
完全固化:必须在200℃~250℃烘烤1 小时
| Typical topcoat | THERMO 600 FINISH LF |
|---|---|
| 适用上涂 | 无铅有机硅耐热面漆600 |
Store in dry, cool condition and away from sources of heat and ignition. Containers
must be kept tightly closed.
贮存于干燥阴凉的环境中,远离热源及火源。包装桶必须保持封闭。
| Shelf life | 12months from date of production (25℃) |
|---|---|
| 贮存期限 | 自生产之日起12 个月(25℃) |
The information given on this sheet is to the best of our knowledge and accurate at
the time of issuing. Since conditions of use are beyond the manufacturer’s control, information contained herein is without warranty, implied or otherwise, and the suitability of the material for the use contemplated is the sole responsibility of the buyer. The information contained on this data sheet is subject to modification at any time due to our policy of modification and product development.Please check this date sheet is current prior to using the product.
本说明书所提供信息均为目前我方所掌握最全面正确的资料,鉴于产品使用条 件非我方所能控制,此中信息不含担保,即仅在选取产品上对买方负责。由 于我公司产品及生产工艺的不断发展,本说明书的内容也会随时进行更改, 此中所有信息均以我方确认为主。产品使用前,请确认所持说明书为最新版 本。
| Issued Date 发行日期 | 2024/10 |
|---|
资料以厂商最新版为准,具体以原厂最新 TDS 为准。查看 关西 KANSAI THERMO 600 PRIMER 有机硅耐热底漆600 原厂 PDF 说明书全文。
原厂包装规格与批次交期以实际供货为准,可联系我们按项目核算。